Sintered Ferrite: Sintered Ferrite; Injected Ferrite; Flexible Ferrite

Hard-ferrite Soft-Ferrite NdFeB SmCo Alnico Pot Magnets Magnetic Products Microwave Ferrite Products
 
Sintered Ferrite
  • Produced from iron oxide and barium carbonate or strontium carbonate

  • Operating temperature range from -40ºC to 250ºC.

  • Very high corrosion resistance.

  • Lowest cost than other permanent magnet.



SPECIFICATION OF SINTERED FERRITE MAGNETS.

 

 

SPECIFICATION OF SINTERED FERRITE MAGNETS.

Material Grade

Remanence

Coercive force

Max. Energy product

Max. Operating temperature

Br

HcB

HcJ

(BH)max

T

T

kG

kA/m

kOe

kA/m

kOe

kJ/m3

MGOe

*Y10T

0.20~0.23

2.0~2.3

135~159

1.7~2.0

223~263

2.8~3.3

8.0~8.8

1.0~1.1

300

Y20

0.36~0.38

3.6~3.8

135~159

1.7~2.0

143~167

1.8~2.1

22.3~25.5

2.8~3.2

300

Y25

0.37~0.39

3.7~3.9

143~159

1.8~2.0

151~167

1.9~2.1

24.7~28.7

3.1~3.6

300

Y26H

0.37~0.39

3.7~3.9

207~223

2.6~2.8

223~238

2.8~3.0

25.5~28.7

3.2~3.6

300

Y30

0.38~0.40

3.8~4.0

159~175

2.0~2.2

167~191

2.1~2.4

27.9~31.0

3.5~3.9

300

Y30H

0.37~0.39

3.7~3.9

191~207

2.4~2.6

231~247

2.9~3.1

27.9~29.5

3.5~3.7

300

Y30H-1

0.38~0.40

3.8~4.0

230~275

2.89~3.45

235~290

2.95~3.65

27.0~32.5

3.39~4.08

300

Y30H-2

0.395~0.415

3.95~4.15

275~300

3.46~3.77

310~335

3.9~4.2

28.5~32.0

3.58~4.02

300

Y35

0.40~0.42

4.0~4.2

223~238

2.8~3.0

231~247

2.9~3.1

31.0~32.6

3.9~4.1

300

Y35H

0.39~0.41

3.9~4.1

238~255

3.0~3.2

247~271

3.1~3.4

28.7~31.0

3.6~3.9

300

Y35H-1

0.37~0.39

3.7~3.9

263~279

3.3~3.5

286~306

3.6~3.8

27.9~30.2

3.5~3.8

300

Y35H-2

0.34~0.36

3.4~3.6

260~290

3.2~3.6

335~350

4.2~4.4

25.0~28.5

3.1~3.6

300

Y44H

0.40~0.44

4.0~4.4

272~304

3.4~3.8

288~320

3.6~4.0

32~35

4.0~4.4

300

* = Isotropic, and others Anisotropic

 